Jgbrown59!
The original, as best I can guess from what original literature I am privy to, was lacquer. I suspect it was supposed to be "gloss", but lacquer tends to "blush", and the rough castings could never be buffed. Engine heat probably didn't help either.
Potmetal Scheblers kept their gloss much better, but the die-castings were much smoother.
I now air-brush a butyrate enamel (forgot whom to thank), which blushes badly without a retarder (especially this time of year!)
But it has withstood P4gas, so far...
....Cotten
The original, as best I can guess from what original literature I am privy to, was lacquer. I suspect it was supposed to be "gloss", but lacquer tends to "blush", and the rough castings could never be buffed. Engine heat probably didn't help either.
Potmetal Scheblers kept their gloss much better, but the die-castings were much smoother.
I now air-brush a butyrate enamel (forgot whom to thank), which blushes badly without a retarder (especially this time of year!)
But it has withstood P4gas, so far...
....Cotten