IMG_1660.jpg Need to know finish of Rocker Arms thanks ulf
Announcement
Collapse
No announcement yet.
Knucklehead 1936 E
Collapse
X
-
Early were nickle wash later copper plated.Be sure to visit;
http://www.vintageamericanmotorcycles.com/main.php
Be sure to register at the site so you can see large images.
Also be sure to visit http://www.caimag.com/forum/
Comment
-
Originally posted by ulfhd View PostOkay i think i understand cooper plated no Problem i jave a late 36 thanks and Happy X MAS for allBe sure to visit;
http://www.vintageamericanmotorcycles.com/main.php
Be sure to register at the site so you can see large images.
Also be sure to visit http://www.caimag.com/forum/
Comment
-
Originally posted by Chris Haynes View PostNote that the wear surfaces were not plated.
It ain't electroplate.
The parts were dipped in molten copper as part of the hardening process, and then the 'wear surfaces' were machined.
Like WLA crankpins, etc.
....CottenAMCA #776
Dumpster Diver's Motto: Seek,... and Ye Shall Find!
Comment