    replied
    Originally posted by Tom Wilcock View Post
    Steve
    Back to the molasses and water rust removal method. I mentioned it to a chemist. The molasses /water mixture simply converts red oxide to black oxide which can be readily removed. It will in no way affect the steel or erode it, only the oxide.
    Tom
    Thanks Tom. I'll side with your chemist.
    I should have written the word "rusty" into my caution. As in:
    If rust is on the hardened surface or high carbon parts ie shafts, gears, clutch hubs, clutch drums, or anything with a bearing race, should not go in the molasses mix?

    I think that a better method for light rust removal of hardened parts is wire buffing.
    Here is another Sporty gear which was in the same box with the other gear and was in similar condition. 10 minutes on the wire wheel and I would use this gear. If I had put it in the molasses mix, the molasses would have chased the oxide reaction which would be present in the rusty areas of the hardened skin of this gear.

    P1120001.jpg

    P1120002.jpg

    P1120003.jpg

    Leave a comment:


  • Tom Wilcock
    replied
    Steve
    Back to the molasses and water rust removal method. I mentioned it to a chemist. The molasses /water mixture simply converts red oxide to black oxide which can be readily removed. It will in no way affect the steel or erode it, only the oxide.
    Tom

    Leave a comment:


  • Steve Little
    replied
    Thanks Bob. I reckon your on the right path. This has a part number finishing in -62. Wikipedia suggested Ranger, Pacer, or Scat for 1962 to 1965.

    FNG1. Man!! That's a weapon. When I was in my mid twenties, I operated tracked machines ie: Koering and Cat feller-bunchers and a Koering processor, in clear fall pine and later on, I was set loose in plantation hard wood.
    I had to have a chainsaw licence to clear the bigger edge trees. I cant think why the guy who built that machine needed all that grunt. Maybe it was for chainsaw racing. That's a mad sport.

    Leave a comment:


  • BigLakeBob
    replied
    Originally posted by Steve Little View Post
    .
    FNG1 I can't identify yours but whatever they are out of, it will most probably have some kind of removable cap to adjust those adjusting screws.
    And these parts are from a similar ammo can in a different part of the world.

    Red lense has TMC-717 SAE-STDB-62 GLO_ BRITE. IT measures 93mm diam or 3 11/16"
    The steel backing plate is 98mm or 3 7/8"


    [ATTACH=CONFIG]23478[/ATTACH]
    DSC06064.JPGDSC06065.JPG
    OD is 95mm and lens configuration looks different. Maybe with this being a NOS in the box with part # might help narrow the search or head you in the right direction. This one says on the bottom 'SAE STDB', on the top 'GUIDE R6-60'. Hole spread is 72mm with 5mm holes offset from center. I bought this hoping it would fit my Leggero, but no cigar.

    https://harleyhummer.com/products/68091-60 Yours looks like this lens, maybe.
    Last edited by BigLakeBob; 01-07-2019, 06:17 PM.

    Leave a comment:


  • T. Cotten
    replied
    Originally posted by Peter Cooke View Post
    I think I read somewhere once that apple cider vinegar works better than white vinegar but I've never got around to trying it.
    It would certainly eat more wallet, Peter!

    I boil some stuff.
    Other stuff you must watch carefully.

    Just don't forget the baking soda neutralization.

    ....Cotten

    Leave a comment:


  • FNG1
    replied
    Hi Steve, no one is interested in the late 50s Triumph Tiger Cub rocker shafts. Check out the Indian Scout motor on this saw.Dow saw.jpg

    Leave a comment:


  • Peter Cooke
    replied
    I think I read somewhere once that apple cider vinegar works better than white vinegar but I've never got around to trying it.

    Leave a comment:


  • Steve Little
    replied
    Hi. Thanks for all the responses, including hard surface, and tempered depths. When we used to make the pressing dies for the frame business, we used to get the heat treatment plant to put a 0015" - 003" skin on them to stop wear.

    Also enjoyed reading the vinegary and tempered responses.

    From my experience, I will throw a note of caution to first time molasses users:
    Hardened or high carbon parts ie shafts, gears, clutch hubs, clutch drums, or anything with a bearing race, should not go in the molasses mix?

    Thanks Pete. I’m off to the super market to see if I can get some good Australian product… Skipping girl vinegar.

    Skipping girl image.jpg

    Leave a comment:


  • Peter Cooke
    replied
    Originally posted by Steve Little View Post
    I would like to try the vinegar next. Is it neat or diluted with water?
    Steve,
    I've used home brand vinegar straight. I figured being home brand it'd be weak anyway without adding any extra water. Works ok, leave it soak for a few days and wire brush off. Good for weed killer as well.

    Leave a comment:


  • T. Cotten
    replied
    Originally posted by Chris Haynes View Post
    Here it is, delivered to your door.
    https://www.amazon.com/YTEX-EQUINE-G...ses+horse+feed
    You are making me a Luddite, Chris!

    Amazon delivered doesn't seem organic, somehow.
    Neither's the 'dollar' store vinegar, but its only a half-block away (and I have no "Amazon" account.. yet.. ).

    Everything has a time and a place, and I'll bet molasses has better effect in some instances than others have in others.
    Pity nobody studies it.

    ....Cotten
    Last edited by T. Cotten; 01-05-2019, 02:36 PM.

    Leave a comment:


  • Chris Haynes
    replied
    Originally posted by T. Cotten View Post
    I'm in a rural town, Chris!
    And still must make a seventy mile round trip to the big city for feed grade molasses.
    Horse owners must be rich. Gotta be.
    ....Cotten
    Here it is, delivered to your door.

    Leave a comment:


  • T. Cotten
    replied
    Originally posted by Chris Haynes View Post
    I have found that Horse feed molasses works best. Buy it at the feed store.
    I'm in a rural town, Chris!

    And still must make a seventy mile round trip to the big city for feed grade molasses.
    Horse owners must be rich. Gotta be.

    So I go through gallons of white vinegar from the "dime-now-dollar" store.
    'Course I use it for many, many other purposes than just converting ferric oxides to soluble ferric acetates.

    Ultimately, it always takes 'elbow grease' or some other mechanical means to remove the crud.

    ....Cotten

    Leave a comment:


  • Chris Haynes
    replied
    I have found that Horse feed molasses works best. Buy it at the feed store.

    Leave a comment:


  • exeric
    replied
    I never put hardened parts, or springs in a chemical bath to remove oxidation. I ruined some parts years ago doing that. I have no idea what happens on a metallurgical level, but I guess acid loves to eat carbon. In regards to the vinegar bath, my method is to make a vinegar to water ratio of about 2 : 1 and monitor the progress. The main reason I use vinegar is because I keep it in a covered bucket behind my storage shed. There is also a large bees nest in a tree back there and I think molasses would be asking for trouble.

    Leave a comment:


  • BigLakeBob
    replied
    In response to the sporty gear and 'some of the hardened skin has dissolved'. I hear quit often remarks like 'going through the hardness'. My experience in the machine shop trade tells me a carburized and hardened piece of mild steel has a hardness thickness of about .035-.060 deep. Whereas a piece of mild steel can be carbo-nitrided to a case hardness of about .015 deep. I am also familiar with gas nitriding (which is very hard- I'd say high 60's Rc) which can be anywhere from .005 to .030 deep, but in my experience the base metal has to be hardened first to at least 28-32Rc. And then there are tool steels which are usually hardened throughout. Do we know how HD parts like gears, crank pins, and shafts were heat treated and what the base metal was?
    Hope I'm not hi-jacking your thread Steve. Thanks, Bob